PF FERROCOLOR ship enamel is applied by spray, brush, roller
The work must be carried out in ventilated areas using personal protective equipment for the skin, respiratory organs, eyes and face.
The preparation of the working composition consists in thorough mixing. If necessary, it is allowed to add a solvent (P4, xylene or white spirit) in an amount of no more than 20%. The working composition not used during the shift should be filled with a small amount of solvent and tightly closed with a factory lid to prevent moisture ingress, gel formation and increased viscosity during storage.
The material can be applied at an air temperature from +5 °C to +35 °C and a relative humidity of up to 85%. It is not allowed to be applied on a wet or wet surface. The material should be applied in a uniform layer with a thickness of 30 to 80 microns, depending on the coating system used. The material is applied in 1-2 layers. The holding time before applying the second layer at a temperature of (20 ± 5) ° C should be at least 8 hours, but not more than 2 days. The thickness of a single–layer coating (on a dry layer) is no more than 30 microns. Approximate consumption rates per layer: from 80 g/m2.